Jan 20, 2026
Laisser un message
Tableau de poids des raccords de tuyauterie forgés Hastelloy C276
|
Taper
|
Poids (kg)
|
|
Classe
|
1/4"
|
3/8"
|
1/2"
|
3/4"
|
1"
|
1 ¼"
|
1 ½"
|
2"
|
2 ½"
|
3"
|
4"
|
|
Coudes à 90 degrés
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Coudes de rue
|
3000
|
0.131
|
0.225
|
0.325
|
0.530
|
0.940
|
1.30
|
1.47
|
2.30
|
|
|
|
|
Coudes à 45 degrés
|
|
|
|
|
|
|
|
|
|
|
|
|
|
T-shirts
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Croix
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Accouplements
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Demi-accouplements
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Casquettes
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Fiches mâles
|
TQ. 3000TE. 6000 TT.
|
|
|
|
|
|
|
|
|
|
|
|
|
Douille hexagonale
|
6000
|
|
|
|
|
|
0.120
|
|
0.150
|
|
0.173
|
|
0.195
|
|
0.214
|
|
|
0.209
|
|
0.280
|
|
0.330
|
|
0.400
|
|
0.480
|
|
|
0.212
|
|
0.314
|
|
0.418
|
|
0.490
|
|
0.540
|
|
|
0.450
|
|
0.513
|
|
0.620
|
|
0.690
|
|
0.704
|
|
|
0.760
|
|
1.14
|
|
1.27
|
|
1.41
|
|
1.53
|
|
|
|
|
Mamelons hexagonaux
|
|
2000 STD-XS
|
|
3000 SCH 160
|
|
6000XXS
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Les syndicats
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Mamelons de tuyau de 100 mm de longueur
|
|
|
|
|
|
|
|
|
|
|
|
|
Poids (kg) des raccords de tuyauterie forgés Hastelloy C276
Taille | Produit (Lbs) |
1/8" |
1/4" |
3/8" |
1/2" |
3/4" |
1" |
1-1/4" |
1-1/2" |
2" |
2-1/2" |
3" |
4" |
| Coude 90 |
3000 |
0.09 |
0.08 |
0.12 |
0.22 |
0.33 |
0.53 |
0.84 |
1.08 |
1.68 |
3.2 |
5.38 |
10.95 |
| 6000 |
0.1 |
0.15 |
0.29 |
0.4 |
0.73 |
1.17 |
1.48 |
2.79 |
3.28 |
|
|
|
| 45 Coude |
3000 |
0.08 |
0.07 |
0.11 |
0.2 |
0.28 |
0.42 |
0.69 |
0.8 |
1.35 |
2.53 |
5.1 |
9.41 |
| 6000 |
0.09 |
0.14 |
0.26 |
0.36 |
0.57 |
0.92 |
1.11 |
2.01 |
2.09 |
|
|
|
| Tee |
3000 |
0.13 |
0.09 |
0.15 |
0.29 |
0.42 |
0.65 |
1.04 |
1.35 |
2.04 |
3.98 |
5.9 |
13.92 |
| 6000 |
0.14 |
0.2 |
0.43 |
0.56 |
0.94 |
1.49 |
1.93 |
3.37 |
3.95 |
|
|
|
| Croix |
3000 |
0.16 |
0.13 |
0.2 |
0.35 |
0.47 |
0.73 |
1.12 |
1.58 |
2.25 |
4.37 |
6.69 |
14.58 |
| 6000 |
0.17 |
0.26 |
0.45 |
0.67 |
1.07 |
1.75 |
2.26 |
3.96 |
4.42 |
|
|
|
| Couplage complet |
3000 |
0.04 |
0.05 |
0.07 |
0.13 |
0.17 |
0.29 |
0.45 |
0.59 |
0.86 |
1.4 |
1.78 |
2.85 |
| 6000 |
0.05 |
0.07 |
0.114 |
0.204 |
0.27 |
0.44 |
0.6 |
1.11 |
1.62 |
|
|
|
| Demi-accouplement |
3000 |
0.04 |
0.05 |
0.07 |
0.13 |
0.21 |
0.3 |
0.34 |
0.66 |
1.09 |
1.63 |
2.1 |
3.71 |
| 6000 |
0.06 |
0.09 |
0.12 |
0.21 |
0.31 |
0.51 |
0.75 |
1.25 |
1.92 |
|
|
|
| Couplage rouge |
3000 |
.04 |
0.05 |
0.07 |
0.13 |
0.19 |
0.27 |
0.49 |
0.59 |
0.97 |
1.42 |
1.88 |
3.31 |
| 6000 |
|
|
|
0.24 |
0.33 |
0.65 |
0.75 |
1.2 |
2.12 |
|
|
|
| Capuchon |
3000 |
0.03 |
0.04 |
0.07 |
0.1 |
0.16 |
0.25 |
0.45 |
0.59 |
0.96 |
.43 |
2.74 |
4.24 |
| 6000 |
0.05 |
0.08 |
0.1 |
0.16 |
0.23 |
0.36 |
0.64 |
0.94 |
1.41 |
|
|
|
| Union |
3000 |
0.28 |
0.28 |
0.25 |
0.35 |
0.49 |
0.81 |
1.1 |
1.61 |
2.16 |
3.5 |
5.15 |
11.59 |
Poids des raccords de tuyauterie à souder à douille forgée en alliage C276
Conforme aux normes ANSI B16.11 et BS 3799, capacité nominale de 3 000 à 6 000 à 9 000 lb
| Produit |
Notation |
1/8" |
1/4" |
3/8" |
1/2" |
3/4" |
1" |
1 1/4" |
1 1/2" |
2" |
2 1/2" |
3" |
4" |
| Coudes à 90 degrés |
3000 livres |
0.08 |
0.08 |
0.12 |
0.24 |
0.29 |
0.48 |
0.75 |
0.95 |
1.65 |
2.50 |
4.30 |
9.70 |
| 6000 livres |
0.15 |
0.17 |
0.30 |
0.43 |
0.66 |
1.14 |
1.60 |
2.70 |
2.95 |
- |
- |
- |
| Coudes à 45 degrés |
3000 livres |
0.08 |
0.08 |
0.10 |
0.19 |
0.25 |
0.38 |
0.58 |
0.83 |
1.15 |
2.05 |
3.40 |
9.00 |
| 6000 livres |
0.12 |
0.12 |
0.24 |
0.30 |
0.53 |
0.86 |
1.07 |
1.90 |
2.35 |
- |
- |
- |
| T-shirts |
3000 livres |
0.12 |
0.12 |
0.19 |
0.31 |
0.40 |
0.58 |
0.91 |
1.25 |
2.10 |
3.15 |
5.25 |
13.50 |
| 6000 livres |
0.21 |
0.21 |
0.40 |
0.56 |
0.91 |
1.41 |
1.75 |
3.56 |
4.10 |
- |
- |
- |
| Croix |
3000 livres |
0.14 |
0.14 |
0.21 |
0.34 |
0.47 |
0.80 |
1.25 |
1.50 |
2.23 |
3.95 |
6.50 |
16.00 |
| 6000 livres |
0.26 |
0.26 |
0.50 |
0.67 |
1.06 |
1.79 |
2.15 |
4.45 |
5.40 |
- |
- |
- |
| Les syndicats |
3000 livres |
0.14 |
0.18 |
0.23 |
0.39 |
0.52 |
0.73 |
1.20 |
1.56 |
2.30 |
5.00 |
7.15 |
| Accouplements |
3000 livres |
0.05 |
0.05 |
0.07 |
0.11 |
0.15 |
0.26 |
0.37 |
0.42 |
0.77 |
1.10 |
1.40 |
2.35 |
| 6000 livres |
0.07 |
0.07 |
0.10 |
0.15 |
0.34 |
0.37 |
0.49 |
0.68 |
1.24 |
- |
- |
- |
| Casquettes |
3000 livres |
0.03 |
0.04 |
0.06 |
0.14 |
0.18 |
0.30 |
0.51 |
0.65 |
0.92 |
1.40 |
2.50 |
3.50 |
| 6000 livres |
0.08 |
0.14 |
0.18 |
0.21 |
0.46 |
0.70 |
0.89 |
1.20 |
- |
- |
- |
| Patron de soudage |
- |
0.20 |
0.23 |
0.29 |
0.38 |
0.53 |
0.83 |
1.31 |
1.86 |
- |
- |
- |
- |
Poids fileté des garnitures de tuyau du nickel C276
B16.11 / BS 3799 Catégorie 2000-3000-6000 lbs
| Produit |
Notation |
1/8" |
1/4" |
3/8" |
1/2" |
3/4" |
1" |
1 1/4" |
1 1/2" |
2" |
2 1/2" |
3" |
4" |
| Coudes à 90 degrés |
2000 livres |
0.08 |
0.08 |
0.11 |
0.23 |
0.28 |
0.46 |
0.80 |
1.00 |
1.60 |
2.30 |
4.35 |
10.25 |
| 3000 livres |
0.14 |
0.14 |
0.27 |
0.37 |
0.60 |
1.08 |
1.22 |
2.45 |
2.50 |
5.25 |
7.40 |
13.00 |
| 6000 livres |
0.31 |
0.31 |
0.50 |
0.69 |
1.25 |
1.65 |
2.75 |
3.22 |
6.25 |
10.00 |
17.00 |
18.00 |
| Coudes à 45 degrés |
2000 livres |
0.10 |
0.10 |
0.11 |
0.21 |
0.24 |
0.39 |
0.70 |
0.85 |
1.23 |
3.00 |
3.50 |
9.00 |
| 3000 livres |
0.13 |
0.13 |
0.25 |
0.36 |
0.53 |
0.78 |
1.02 |
1.70 |
2.35 |
5.40 |
6.00 |
10.50 |
| 6000 livres |
0.25 |
0.25 |
0.35 |
0.60 |
0.95 |
1.22 |
1.35 |
2.55 |
5.60 |
8.00 |
15.50 |
13.00 |
| T-shirts |
2000 livres |
0.12 |
0.12 |
0.18 |
0.29 |
0.39 |
0.55 |
0.93 |
1.30 |
1.80 |
3.00 |
5.50 |
14.00 |
| 3000 livres |
0.21 |
0.21 |
0.31 |
0.49 |
0.80 |
1.31 |
1.61 |
3.20 |
3.55 |
6.50 |
9.25 |
17.00 |
| 6000 livres |
0.41 |
0.41 |
0.60 |
0.94 |
1.59 |
2.14 |
3.39 |
4.50 |
10.00 |
13.00 |
19.50 |
18.00 |
| Croix |
2000 livres |
0.14 |
0.14 |
0.19 |
0.34 |
0.42 |
0.75 |
1.15 |
1.45 |
2.25 |
4.50 |
7.15 |
15.00 |
| 3000 livres |
0.22 |
0.22 |
0.40 |
0.63 |
0.99 |
1.63 |
1.97 |
3.70 |
4.90 |
10.50 |
11.50 |
21.70 |
| 6000 livres |
0.45 |
0.45 |
0.70 |
1.16 |
1.80 |
2.50 |
4.10 |
5.20 |
12.30 |
14.00 |
25.00 |
23.00 |
| Accouplements |
3000 livres |
0.05 |
0.05 |
0.06 |
0.14 |
0.20 |
0.39 |
0.73 |
1.03 |
1.35 |
2.30 |
3.15 |
5.80 |
| 6000 livres |
0.10 |
0.10 |
0.12 |
0.37 |
0.45 |
1.00 |
1.65 |
1.85 |
2.80 |
4.00 |
5.50 |
10.00 |
| Demi-accouplements |
3000 livres |
0.02 |
0.03 |
0.03 |
0.07 |
0.11 |
0.20 |
0.37 |
0.51 |
0.666 |
1.15 |
1.57 |
2.90 |
| 6000 livres |
0.04 |
0.05 |
0.06 |
0.19 |
0.23 |
0.50 |
0.83 |
0.92 |
1.40 |
2.00 |
2.75 |
5.00 |
| Casquettes |
3000 livres |
0.04 |
- |
0.05 |
0.16 |
0.06 |
0.20 |
0.13 |
0.29 |
0.21 |
0.40 |
0.37 |
0.70 |
| 6000 livres |
0.60 |
1.10 |
0.73 |
1.35 |
1.10 |
2.10 |
2.31 |
3.50 |
3.00 |
4.80 |
4.50 |
7.50 |
| Coudes de rue |
3000 livres |
- |
0.13 |
0.23 |
0.33 |
0.53 |
0.94 |
1.30 |
1.47 |
2.30 |
- |
- |
- |
| Patron de soudage |
- |
0.20 |
0.23 |
0.29 |
0.38 |
0.53 |
0.83 |
1.31 |
1.86 |
- |
- |
- |
- |
| Mamelon de tuyau - 100 mm |
3000 (XS) |
0.07 |
0.08 |
0.11 |
0.16 |
0.22 |
0.31 |
0.44 |
0.53 |
0.74 |
1.12 |
1.46 |
2.15 |
| |
6000 (XXS) |
- |
- |
- |
0.25 |
0.36 |
0.54 |
0.77 |
0.95 |
1.31 |
2.00 |
2.65 |
4.00 |
| Prise - Tête Carrée |
- |
0.01 |
0.02 |
0.03 |
0.05 |
0.09 |
0.17 |
0.27 |
0.40 |
0.60 |
0.89 |
1.25 |
3.10 |
| Bouchon - Tête ronde |
- |
0.04 |
0.05 |
0.07 |
0.13 |
0.22 |
0.32 |
0.50 |
0.72 |
1.35 |
2.20 |
3.30 |
6.00 |
| Bouchon - tête hexagonale |
- |
0.02 |
0.03 |
0.05 |
0.07 |
0.13 |
0.22 |
0.41 |
0.49 |
0.77 |
1.16 |
1.94 |
4.50 |
| Syndicats FF |
3000 livres |
0.14 |
0.17 |
0.21 |
0.31 |
0.49 |
0.83 |
1.22 |
1.53 |
2.30 |
5.00 |
6.25 |
- |
| |
6000 livres |
0.20 |
0.30 |
0.50 |
1.12 |
1.60 |
2.15 |
2.42 |
4.73 |
6.50 |
9.50 |
19.20 |
- |
| Syndicats MF |
3000 livres |
0.16 |
0.21 |
0.27 |
0.46 |
0.61 |
0.99 |
1.55 |
1.90 |
2.90 |
- |
- |
- |
| Douille à tête hexagonale |
- |
0.02 |
0.03 |
0.06 |
0.10 |
0.17 |
0.33 |
0.42 |
0.62 |
1.27 |
1.65 |
3.10 |
- |
| Mamelons hexagonaux |
- |
0.02 |
0.03 |
0.06 |
0.08 |
0.15 |
0.24 |
0.37 |
0.45 |
- |
- |
- |
- |
| Mamelons à sertir |
Plaine |
0.04 |
0.05 |
0.09 |
0.14 |
0.17 |
0.32 |
0.49 |
0.60 |
0.93 |
- |
- |
- |
| Vissé |
- |
0.17 |
0.22 |
0.29 |
0.33 |
0.50 |
0.75 |
0.95 |
1.60 |
2.10 |
- |
- |
- |
Vérifiez les prix d'aujourd'hui pour les raccords de tuyauterie forgés chinois Hastelloy C276
Nous fournissons également des raccords de tuyauterie à souder par emboîtement Hastelloy C276 aux meilleurs prix. Vous pouvez consulter notre dernière liste de prix pour les raccords de tuyauterie forgés Hastelloy C-22 de différentes tailles. Contactez Gnee Steel dès maintenant pour obtenir le meilleur devis sur les coudes forgés Hastelloy C22.
Téléphone : +8615824687445
E-mail:ss@gneesteel.com