Dimensions et informations de tolérance pour les barres rondes en alliage 601

Dimensions standard de la barre ronde Inconel 601

Diamètre ou
Largeur
(mm)
Poids par mètre Zone sectionnelle Périmètre
  Carré
(kg)
Rond
(kg)
Carré
(cm²)
Rond
(cm²)
Carré
(cm)
Rond
(cm)
5.0 0.20 0.15 0.25 0.20 2.0 1.57
5.5 0.24 0.19 0.30 0.24 2.2 1.78
6.0 0.28 0.22 0.36 0.28 2.4 1.88
7.0 0.38 0.30 0.49 0.38 2.8 2.20
8.0 0.50 0.39 0.64 0.50 3.2 2.51
9.0 0.64 0.50 0.81 0.64 3.6 2.83
10 0.73 0.63 1.00 0.79 4.0 3.14
11 0.95 0.75 1.21 0.95 4.4 3.46
12 1.13 0.89 1.44 1.13 4.8 3.77
14 1.54 1.21 1.96 1.54 5.6 4.40
16 2.01 1.58 2.56 2.01 6.4 5.03
18 2.54 2.00 3.24 2.54 7.2 5.65
20 3.14 2.47 4.00 3.14 8.0 6.28
22 3.80 2.98 4.84 3.80 8.8 6.91
25 4.91 3.85 6.25 4.91 10.0 7.85
28 6.15 4.83 7.84 6.16 11.2 8.80
32 8.04 6.31 10.24 8.04 12.8 10.05
36 10.17 7.99 12.96 10.18 14.4 11.31
40 12.56 9.86 16.00 12.57 16.0 12.57
45 15.90 12.49 20.25 15.90 18.0 14.14
50 19.62 15.41 25.00 19.64 20.0 15.71
56 24.62 19.34 31.36 24.63 22.4 17.59
63 31.16 24.47 36.69 31.17 25.2 19.79
71 39.57 31.08 50.41 39.59 28.4 22.31
80 50.24 39.46 64.00 50.27 32.0 25.13

 

Tolérance de barre ronde brillante Inconel UNS N06601

Tolérance des barres rondes Inconel 601 série ISO "H" en MM
Taille (mm) H12 H11 H10 H9 H8 H7 H6 H5
Plus de 180 - 250 +0.46/0 +0.29/0 +0.185/0 +0.115/0 +0.072/0 +0.046/0 +0.029/0 +0.02/0
Plus de 120 - 180 +0.4/0 +0.25/0 +0.16/0 +0.1/0 +0.063/0 +0.04/0 +0.025/0 +0.018/0
Plus de 80 - 120 +0.35/0 +0.22/0 +0.14/0 +0.087/0 +0.054/0 +0.035/0 +0.022/0 +0.015/0
Plus de 50 - 80 +0.3/0 +0.19/0 +0.12/0 +0.074/0 +0.046/0 +0.03/0 +0.019/0 +0.013/0
Plus de 30 - 50 +0.25/0 +0.16/0 +0.1/0 +0.062/0 +0.039/0 +0.025/0 +0.016/0 +0.011/0
Plus de 18 - 30 +0.21/0 +0.13/0 +0.084/0 +0.052/0 +0.033/0 +0.021/0 +0.013/0 +0.009/0
Plus de 10 - 18 +0.18/0 +0.11/0 +0.07/0 +0.043/0 +0.027/0 +0.018/0 +0.011/0 +0.008/0
Plus de 6 - 10 +0.15/0 +0.09/0 +0.058/0 +0.036/0 +0.022/0 +0.015/0 +0.009/0 +0.006/0
Plus de 3 - 6 +0.12/0 +0.075/0 +0.048/0 +0.03/0 +0.018/0 +0.012/0 +0.008/0 +0.005/0
~ à 3 +0.1/0 +0.06/0 +0.04/0 +0.025/0 +0.014/0 +0.01/0 +0.006/0 +0.004/0

 