Épaisseur de la plaque d'acier Inconel 600, épaisseur de la plaque métallique en alliage 600 (mm), épaisseur de la plaque d'acier en alliage de nickel 600, épaisseur de la plaque d'acier UNS N06600 (mm).
Tableau d'épaisseur de feuille Uns N06600
| Jauge (ga) | Épaisseur de l'acier (po) | Épaisseur de l'acier (mm) | Épaisseur de l'aluminium (po) | Épaisseur de l'aluminium (mm) |
| 3 | 0.2391 | 6.07 | 0.2294 | 5.83 |
| 4 | 0.2242 | 5.69 | 0.2043 | 5.19 |
| 5 | 0.2092 | 5.31 | 0.1819 | 4.62 |
| 6 | 0.1943 | 4.94 | 0.162 | 4.11 |
| 7 | 0.1793 | 4.55 | 0.1443 | 3.67 |
| 8 | 0.1644 | 4.18 | 0.1285 | 3.26 |
| 9 | 0.1495 | 3.80 | 0.1144 | 2.91 |
| 10 | 0.1345 | 3.42 | 0.1019 | 2.59 |
| 11 | 0.1196 | 3.04 | 0.0907 | 2.30 |
| 12 | 0.1046 | 2.66 | 0.0808 | 2.05 |
| 13 | 0.0897 | 2.28 | 0.072 | 1.83 |
| 14 | 0.0747 | 1.90 | 0.0641 | 1.63 |
| 15 | 0.0673 | 1.71 | 0.0571 | 1.45 |
| 16 | 0.0598 | 1.52 | 0.0508 | 1.29 |
| 17 | 0.0538 | 1.37 | 0.0453 | 1.15 |
| 18 | 0.0478 | 1.21 | 0.0403 | 1.02 |
| 19 | 0.0418 | 1.06 | 0.0359 | 0.91 |
| 20 | 0.0359 | 0.91 | 0.032 | 0.81 |
| 21 | 0.0329 | 0.84 | 0.0285 | 0.72 |
| 22 | 0.0299 | 0.76 | 0.0253 | 0.64 |
| 23 | 0.0269 | 0.68 | 0.0226 | 0.57 |
| 24 | 0.0239 | 0.61 | 0.0201 | 0.51 |
| 25 | 0.0209 | 0.53 | 0.0179 | 0.45 |
| 26 | 0.0179 | 0.45 | 0.0159 | 0.40 |
| 27 | 0.0164 | 0.42 | 0.0142 | 0.36 |
| 28 | 0.0149 | 0.38 | 0.0126 | 0.32 |
| 29 | 0.0135 | 0.34 | 0.0113 | 0.29 |
| 30 | 0.012 | 0.30 | 0.01 | 0.25 |
| 31 | 0.0105 | 0.27 | 0.0089 | 0.23 |
| 32 | 0.0097 | 0.25 | 0.008 | 0.20 |
| 33 | 0.009 | 0.23 | 0.0071 | 0.18 |
| 34 | 0.0082 | 0.21 | 0.0063 | 0.16 |
| 35 | 0.0075 | 0.19 | 0.0056 | 0.14 |
| 36 | 0.0067 | 0.17 | – | – |
Tableau d'épaisseur de plaque en alliage 600
| Jauge | LB/Sq. Fort. | LB/po². | Tolérance de jauge de plaque | ||
| 72″ de large | 96″ de large | ||||
| 3/16 | 0.1875 | 8.579 | 0.05958 | +.045″ -.010″ | +.050″ -.010″ |
| 7/32 | 0.2187 | 9.870 | 0.06854 | ||
| 1/4 | 0.2500 | 11.162 | 0.07750 | ||
| 5/16 | 0.3125 | 13.746 | 0.09546 | ||
| 3/8 | 0.3750 | 16.496 | 0.11456 | +.055″ -.010″ | +.060″ -.010″ |
| 7/16 | 0.4375 | 19.080 | 0.13250 | ||
| 1/2 | 0.5000 | 21.633 | 0.15044 | ||
| 9/16 | 0.5625 | 24.247 | 0.16838 | ||
| 5/8 | 0.6250 | 26.831 | 0.18633 | ||
| 11/16 | 0.6875 | 29.415 | 0.20427 | ||
| 3/4 | 0.7500 | 32.123 | 0.22308 | +.060″ -.010″ | +.065″ -.010″ |
| 13/16 | 0.8125 | 34.707 | 0.24102 | ||
| 7/8 | 0.8750 | 37.291 | 0.25897 | ||
| 15/16 | 0.9375 | 39.875 | 0.27691 | ||
| 1 | 1.0000 | 42.665 | 0.29628 | +.070″ -.010″ | +.075 -.010″ |
| 1-1/8 | 1.1250 | 47.833 | 0.33217 | ||
| 1-1/4 | 1.2500 | 53.001 | 0.36806 | ||
| 1-3/8 | 1.3750 | 58.169 | 0.40395 | ||
| 1-1/2 | 1.5000 | 63.337 | 0.43984 | ||
| 1-3/4 | 1.7500 | 73.672 | 0.51161 | ||
| 2 | 2.0000 | 84.008 | 0.58339 | +.125″ -.010″ | +.150″ -.010″ |
| 2-1/8 | 2.1250 | 89.610 | 0.62229 | ||
| 2-1/4 | 2.2500 | 94.777 | 0.65817 | ||
| 2-1/2 | 2.5000 | 105.113 | 0.72995 | ||
| 2-3/4 | 2.7500 | 115.449 | 0.80173 | ||
| 3 | 3.0000 | 126.301 | 0.87709 | +.150″ -.010″ | +.160″ -.010″ |
| 3-1/2 | 3.5000 | 146.972 | 1.02064 | ||
| 4 | 4.0000 | 168.264 | 1.16850 | +.180″ -.010″ | +.200″ -.010 |
Tableau d'épaisseur de bobine de nickel 600
| Épaisseur (mm) | 1000 Inférieur ou égal à Largeur < 1250 (mm) | 630 Inférieur ou égal à Largeur < 1000 (mm) | 1250 Inférieur ou égal à Largeur < 1550 (mm) |
| 0,40 Inférieur ou égal à T < 0,60 | ±0.035 | ±0.035 | - |
| 1,25 Inférieur ou égal à T < 1,60 | ±0.060 | ±0.055 | ±0.060 |
| 1,60 Inférieur ou égal à T < 2,00 | ±0.070 | ±0.065 | ±0.080 |
| 0,25 Inférieur ou égal à T < 0,40 | ±0.035 | ±0.030 | - |
| 0,80 Inférieur ou égal à T < 1,00 | ±0.050 | ±0.040 | ±0.050 |
| 0,60 Inférieur ou égal à T < 0,80 | ±0.040 | ±0.040 | - |
| 1,00 Inférieur ou égal à T < 1,25 | ±0.055 | ±0.050 | ±0.060 |

ss@gneesteel.com
Consultez les dimensions des plaques d'acier Inconel 600 (mm), les tailles de plaques standard et les tailles de bobines, le tableau des tailles de bobines et les dimensions des plaques d'acier inoxydable Gnee Steel.